Susceptibility of titanium alloys to hot-salt stress-corrosion cracking increased as follows: Ti-2Al-11Sn-5Zr-0.2Si(679), Ti-6Al-2Sn-4Zr-2Mo(6242), Ti-6Al-4V(64), Ti-6Al-4V-3Co(643), Ti-8Al-1Mo-1V(811), and Ti-13V-11Cr-3A1(13-11-3). The Ti-5Al-6Sn-2Zr-1Mo-0.25Si(5621S) alloy was both the least and most susceptible depending on heat treatment. Such rankings can be drastically altered by heat-to-heat and processing variations. Residual compressive stresses and cyclic exposures also reduce susceptibility to stress-corrosion. Simulated turbine-engine compressor environmental variables such as air velocity, pressure, dewpoint, salt concentration, and salt deposition temperature have only minor effects. Detection of substantial concentrations of hydrogen in all corroded alloys confirmed the existence of a hydrogen embrittlement mechanism.--P. [i].


Materials Properties Handbook

Materials Properties Handbook

Author: Gerhard Welsch

Publisher: ASM International

Published: 1993-12-31

Total Pages: 1206

ISBN-13: 9780871704818

DOWNLOAD EBOOK

Comprehensive datasheets on more than 60 titanium alloys More than 200 pages on metallurgy and fabrication procedures Input from more than 50 contributors from several countries Careful editorial review for accuracy and usefulness. Materials Properties Handbook: Titanium Alloys provides a data base for information on titanium and its alloys, and the selection of specific alloys for specific applications. The most comprehensive titanium data package ever assembled provides extensive information on applications, physical properties, corrosion, mechanical properties (including design allowances where available), fatigue, fracture properties, and elevated temperature properties. The appropriate specifications for each alloy are included. This international effort has provided a broad information base that has been compiled and reviewed by leading experts within the titanium industry, from several countries, encompassing numerous technology areas. Inputs have been obtained from the titanium industry, fabricators, users, government and academia. This up-to-date package covers information from almost the inception of the titanium industry, in the 1950s, to mid-1992. The information, organized by alloy, makes this exhaustive collection an easy-to-use data base at your fingertips, which generally includes all the product forms for each alloy. The 60-plus data sheets supply not only extensive graphical and tabular information on properties, but the datasheets also describe or illustrate important factors which would aid in the selection of the proper alloy or heat treatment. The datasheets are further supplemented with back-ground information on the metallurgy and fabrication characteristics of titanium alloys. An especially extensive coverage of properties, processing and metallurgy is provided in the datasheet for the workhorse of the titanium industry, Ti-6Al-4V. This compendium includes the newest alloys made public. even those still under development. In many cases, key references are included for further information on a given subject. Comprehensive datasheets provide extensive information on: Applications, Specifications, Corrosion, Mechanical Design Properties, Fatigue and Fracture


Stress-corrosion Cracking

Stress-corrosion Cracking

Author: Russell H. Jones

Publisher: ASM International(OH)

Published: 1992

Total Pages: 466

ISBN-13:

DOWNLOAD EBOOK

Details the many conditions under which stress-corrosion cracking (SCC) can occur, the parameters which control SCC, and the methodologies for mitigating and testing for SCC, plus information on mechanisms of SCC with experimental data on a variety of materials. Contains information about environmen


Titanium and Titanium Alloys

Titanium and Titanium Alloys

Author: Christoph Leyens

Publisher: John Wiley & Sons

Published: 2006-03-06

Total Pages: 532

ISBN-13: 3527605207

DOWNLOAD EBOOK

This handbook is an excellent reference for materials scientists and engineers needing to gain more knowledge about these engineering materials. Following introductory chapters on the fundamental materials properties of titanium, readers will find comprehensive descriptions of the development, processing and properties of modern titanium alloys. There then follows detailed discussion of the applications of titanium and its alloys in aerospace, medicine, energy and automotive technology.